FBRT-W304L-21/2-11/2-10S

Please register/login to check stock and price information

Reducing Tees

Pipe dimensions

Nominal Diameter, Run side, Inch:
21/2
Nominal Diameter, Run side, mm:
73.03
Nominal Diameter, Branch side, Inch:
11/2
Nominal Diameter, Branch side, mm:
48.26
Wall Thickness, Inch:
10S
Wall Thickness, mm:
3.05

Product data

Unit weight (kg/piece):
0.90

Product Standards

  • ASTM A 403 / ASME SA 403
  • Dimensions as per ASME B16.9
  • Bevelled ends as per ASME B16.25
  • NACE MR0175 / MR0103, ISO 15156

These fittings are externally sourced from reputed manufaturers and will be supplied from our Venlo, Nethelands warehouse. Please contact our sales support team for complete details on product specification and standards.