| Catalogue code | Outside Diameter, inch | Pressure rating, Lbs | Stock |
|---|---|---|---|
| FFB-316L-1/2-150-EU | 1/2 | 150 | |
| FFB-316L-3/4-150-EU | 3/4 | 150 | |
| FFB-316L-1-150-EU | 1 | 150 | |
| FFB-316L-11/2-150-EU | 11/2 | 150 | |
| FFB-316L-2-150-EU | 2 | 150 | |
| FFB-316L-3-150-EU | 3 | 150 | |
| FFB-316L-4-150-EU | 4 | 150 | |
| FFB-316L-6-150-EU | 6 | 150 |