THR-310H-3/8-SCH40

Please register/login to check stock and price information

Pipe dimensions

Nominal Diameter, inch:
3/8
Nominal Diameter, mm:
17.15
Wall Thickness, Inch:
40S
Wall Thickness, mm:
2.31

Product data

Unit weight (kg/meter):
0.84

Product Standards

  • ASTM A312/ASME SA312
  • EN 10297-2
  • EN 10216-5 TC1
  • NACE MR0175/ISO 15156