THR-E-7RE10-1-SCH80

Please register/login to check stock and price information

Pipe dimensions

Nominal Diameter, inch:
1
Nominal Diameter, mm:
33.4
Wall Thickness, Inch:
80S
Wall Thickness, mm:
4.55

Product data

Unit weight (kg/meter):
3.28

Product Standards

  • ASTM A312/ASME SA312
  • EN 10297-2
  • EN 10216-5 TC1
  • NACE MR0175/ISO 15156