Pipe dimensions
Nominal Diameter, inch:
Nominal Diameter, mm:
60.3
Wall Thickness, Inch:
Wall Thickness, mm:
3.65
Product data
Unit weight (kg/meter):
5.16
Product Standards
ASTM A312/ASME SA312
EN 10297-2
EN 10216-5 TC1
NACE MR0175/ISO 15156