MBR-SAF32760+-1 1/8

Please register/login to check stock and price information

Dimensions

Outside Diameter, mm:

Product data

Unit weight (kg/meter):
5.13

Product Standards

  • ASTM A479/ASTM A276,NORSOK MDS D57 Rev 6
  • ISO 17781:2017:QL1,IOGP S-563:2018
  • EN 10088-3, EN 10088-5, ISO 15156-3
  • Length 3-6.5 meters,Tolerance -0/+0.25mm