TS-304L-12-10S

Please register/login to check stock and price information

Pipe dimensions

Nominal Diameter, inch:
12
Nominal Diameter, mm:
323.85
Wall Thickness, Inch:
10S
Wall Thickness, mm:
4.57

Product data

Unit weight (kg/meter):
36.54

Product Standards

  • ASTM A 312 / ASME SA 312, ASTM A 999
  • EN 10216-5 TC1, NACE MR0175 / MR0103
  • ISO 15156, random lengths 5 - 7 meters
  • Tolerances as per ASME B36.19,plain ends