- ASTM A 312 / ASME SA 312, ASTM A 999
- EN 10216-5 TC1, NACE MR0175 / MR0103
- ISO 15156, random lengths 5 - 7 meters
- Tolerances as per ASME B36.19,plain ends
TS-316L-10-40S
Pipe dimensions
- Nominal Diameter, inch:
- 10
- Nominal Diameter, mm:
- 273.05
- Wall Thickness, Inch:
- 40S
- Wall Thickness, mm:
- 9.27
Product data
- Unit weight (kg/meter):
- 61.22