MBR-SANMAC316L-10

Please register/login to check stock and price information

Solid Round Bar

Dimensions

Outside Diameter, mm:
254

Product data

Unit weight (kg/meter):
411.20

Product Standards

  • ASTM A479 / ASTM A276, EN 10088-5
  • EN 10272,EN 10222-5,AD2000-W2,EN 10088-3
  • NORSOK MDS S01 REV 4 / NACE MR 0175
  • Stock random length 5000 to 7000 mm

These round bars will be supplied from our Sandviken, Sweden warehouse