TWH-304L-18-10S

Please register/login to check stock and price information

Pipe dimensions

Nominal Diameter, inch:
18
Nominal Diameter, mm:
457.2
Wall Thickness, Inch:
10S
Wall Thickness, mm:
4.78

Product data

Unit weight (kg/meter):
54.15

Product Standards

  • ASTM A 312 / ASME SA 312, ASTM A 999
  • Tolerances as per B36.19
  • NACE MR0175 / MR0103, ISO 15156
  • Stock fix lengths 6000 mm